Originally Posted by jeremy_smitty View Post
I got the powder from my powdercoater...I think he uses tiger drylac. I apply it when the parts are hot or cold, doesn't make that big of a difference. I think I am going to try applying the powder to the parts when they are cold, placing them in a cold oven, and then slowly creep up on the temperature until the part flows out and reaches temp. Maybe I can do two coats instead of one coat to prevent runs...no? I have the oven at 375, which are the specs on the powder.
it looks like the problem is probably when you apply the powder (too thick)