Polishing Questions
I recently purchased the polishing kit from Caswell for Aluminum. I used a die grinder with about 26,000 rpm. First off I had trouble getting the block of compound onto the wheel. It seemed to just decinegrate when I ran the wheel up to it. I set it out in the sun and that seemed to help alittle, but there still wasnt much compound on the wheel. Also, I couldn't get the aluminum to show any results. It honestly didn't look any different from when I started. I used the black compound with the rope like wheel. Does anyone have any tips? Is the grinder fast enough? I really appreciate any help, I want to get my bike done for the sand dunes during Thanksgiving!!!
Shane
|