Default What am i doing wrong?? Green drab

Ok, i tryed everything i could, i opened up the package, 2 gal. of distilled water, mixed both A & b together, solution came out yellow?? took out my heater and heated to 80 degree,s then to 85, copy caded some small parts, came out awesome, then when i put them into the green drab solution they are as yellow as the yellow cad solution, ive tryed differant temps, within 5 degrre,s, this cannot be this hard so what gives here?? frustrated?? Don,t you think the drab solution would look green?? HELP!!!