Re: Double Coat
Another method that has been used for second coats, is to cure it and pull it from the oven and let it get down to around 180 deg and hot flock it. But be careful with hot flocking or you can get to much powder on on it. It starts to flow as you spray.
Otherwise cure the first coat and let it cool and just spray the second coat. Make sure you have a good ground on the part
What gun do you have?
__________________
Who says you can't teach an ole dog new tricks?
|