You might check with Glyptal. I think they make a couple of thinners. G1500 comes to mind but you'll need to check. There's a couple depending on what "paint" you're using. According to the MSDS sheet for G1500, it's made from a 60/40 blend of Xylene and Naphtha, respectively.