Default Re: Greaseless compound leaving "orange peel"

Use a little white compound on the wheel after the greaselss dries. Re-apply as needed.

2 hours is a bit excessive. You should be able to use it right away if the heat gun hardens it up, just make sure it's not still soft underneath.