Greaseless compound leaving "orange peel"
View Single Post
#
5
(
permalink
)
02-10-2008, 05:24 PM
mpierich
Metal Finishing Guru
Join Date: Aug 2004
Posts: 713
Re: Greaseless compound leaving "orange peel"
I guarantee that the orangepeeel is from the greaseless, and that the white compound prevents 90% of it.