Quote:
Originally Posted by mikmj View Post
Unless you blast outside you still have the sand dust in the air.........




Mike
That's why the best protection you can get is a supplied air system that will pump in air under a hood or mask and eliminate any chance of breathing in any of that junk.I am soon to get one and must say i will be using it everytime i sandblast,even if i am outside.