I have an antique silver coin that is set in a silver ring with four very small tabs holding the coin in place,this is a necklace charm,my customer wants the ring and hoop regold plated but not the coin in the center ,he wants that to be kept original,and no I cant remove the coin without damaging the small silver tabs .