I have found the best source of un-coated copper wire in varying guages is to simply get hold of standard domestic electrical wiring from the hrdware store. Better still go to a scrap merchant and buy it second hand.. Even better if you have legal access to a demolition site(freebie). And no I don't mean knocking it off. LOL

Just depends how much you need.