"hook the chrome piece to the positive terminal, and place a swab covered anode on the negative end. You then place the swab in the solution (sodium hydroxide I believe) and then stroke the chrome plated piece. The chrome will then come off slowly"

Is there anywhere I can find detailed instructions on this process? What is the swab made of?

How quickly is it supposed to work? I have the caswell stripper but the lable was damaged so I cant see the instructions...