View Single Post
  #4 (permalink)  
Old 02-18-2008, 11:10 PM
CarWiz's Avatar
CarWiz CarWiz is offline
Experienced Metal Finisher
 
Join Date: Sep 2005
Location: South Texas
Posts: 353
CarWiz is an unknown quantity at this point
Default Re: Electroless Nickel Post Heat?

I use 400-450F. I would want to know what the base metal might be if they are using 400C. That could be for stainless steel or some specialized process. My information says 400F is enough. You sure don't want to bake many of the die-cast alloys at your temp or you'll end up with the part all over the inside of your oven.
Reply With Quote