Well, ok, ive tryed everything now, spent 4 hrs today, cleaning recleaning carbuator arms trying to get the olive drab to work, tryed 20 min. to 25 min in the copy cad solution, took parts out, looked great, put them into grren drab solution with horrible results, i am going to try and post a picture, temp at 80 degrree,s the 85 with no better results!! Someone please help me out!!
|