Default Re: What did we do wrong?

Desmut will cause large crater pits that you will not be able to directly see until the parts are prepped or attempted to be anodized. It seems to create a bubble pit sort of which doesnt show its ugly head til the top metal has been removed. Ive only seen this happen to parts left in desmutting chemicals overnight though.