http://www.caswellplating.com/kits/ph_tester.html
overtime the ph will start to steer up or down and the ph reading will be inaccurate. so you have to get some buffer solution to calibrate the tester.
just order some of the PH 4.0 Buffer Solution, also get ph 7.0 buffer solution.