View Single Post
  #2 (permalink)  
Old 02-21-2008, 03:01 PM
acidrain acidrain is offline
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 833
acidrain is on a distinguished road
Default Re: evaporating acid

Unless it's been leaking, it's just the water that is disapearing. You can safely add water slowly to the mix. It will generate some heat, so be careful... use cool, distilled water and wear eye protection.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote