Regarding a peak detection method; a method of peak detection that is dead S L O W is required. This isn't easy to do with analog peak detectors, I was thinking about a software method. At the lower LCD current densities, if it takes you less than maybe 15 minutes to decide that the peak has been reached, you are going too fast, and might be fooled. Look at the time scale in the anodization curves.