Default Re: I just can't figure this out.

Something with your dye process I'll guess. Were the parts touching each other or the sides of the tank either during dye or sealing? They have to hang so they don't touch.
How about after dye? Were the parts allowed to dry or lay on a towel or something?
After dyeing, let them hang in a rinse tank, or rinse and go directly to sealer.