Re: New Oven
The coil is a two pole, 120v, 55amp definate purpose contactor purchased at the same appliance parts supplier as the elements. The one we used costed between 50 and 60 dollars. The appliance supplier will ask for the model number for your appliance but just tell them to give you cheap two pole coil to step up your voltage to 240. The timer is just a cheap digital kitchen timer that uses a AA battery available just about everywhere.
|