Hey whats up everyone! I am pretty new at the coating industry but I am just asking all the stupid questions to learn so please HELP!
I was just wondering how the whole two coat process works? If I wanted to do something two colors would I just coat the part one color, bake it and let it cool then tape it off and coat it another color? I have found that applying a second coat is hard when the part is not hot. If I let the part cool and try to spray the second color the powder doesnt seem to want to stick to it and if it does it is not and even coat. I usually just prebake the part and spray it while it is still warm but I get worried because it will start to flow and I dont know if the coat is even.
Any suggestions or even if you have time by telling me your process It would help out soooo much! Thanks!