View Single Post
  #4 (permalink)  
Old 02-24-2008, 08:23 AM
carts69 carts69 is offline
Newbie
 
Join Date: Nov 2007
Posts: 48
carts69 is an unknown quantity at this point
Default Re: Copper plating question

Quote:
Originally Posted by carts69 View Post
Hi... The base metal is steel, prior to plating its polished, de-greased in sd175,i don't activate the steel is the correct?
forgot to mention i flash copper plated with brush plate copper prior to acid copper tank, although this has happened with plating onto nickel.What is this build up of copper sludge on part & hanging wire
Reply With Quote