Default Re: How do you powder coat two different colors with a nice sharp edge

Quote:
Originally Posted by CarWiz View Post
Shoot the letter color first and bake. Mask the letters using high temp tape then shoot the background color. Bake just long enough to set the background color (so you don't knock it off), cool then remove the tape. Return it to the oven and complete the bake. This is reverse of how the plate was painted but it's easier to use the width of the tape as the letters than trying to mask the background.
I think this would be hard to do around the outer edge and large letters but next to impossible on the small New York letters?
__________________
Glenn R. Lever
Rochester, New York 14617-2012
My Cars http://www.leverfamilysite.com/vehicles.htm
Control arm Info http://www.leverfamilysite.com/GM_A_body.htm

Join us July 6-8, 2007 for the 5th Annual Northern Chevelle Gathering, Niagara Falls, NY!!!
Reply With Quote