That sounds like the amps are too high. (cloudy/streaking) Also watch that you don't contaminate your chemicals with zinc. Using zinc coated wire (for hanging or connecting) or utensils can ruin a whole batch of chemicals.
It's important to accurately calculate the surface area of part(s) to be plated as the amps are given as per/square inch. Keep us posted on your tests.
|