I have a 3 2800 watt elements a 40amp breaker,10 gage wire,so far I've blown 2 40amp ssr's and 2 60amp ssr's,my wiring is the same as the wiring diagram posted on this forum,after using more heat sink on the 2nd 60amp ssr I set the oven for 150 degrees,it shut of then when the temp dropped below 150 it came back on but never shut off again,my ssr seems to shorted on the load side,although I can run my oven it won't shut off,HELP PLEASE!