Re: Just made 40 Titanium spring wire clips
They are very good, They are however, twice the diameter of his. They will give a strong hold, but if your doing small parts thick wire isnt going to help you. I can do $2.50 a foot plus shipping, and can cut it shorter for easier shipping.