Unhappy Parts won't even anodize?!?!

Hey guys,

I just tryed to anodize my first part and it went fine I just left it in there for 15 min not the recomened 90min. So after figuring out if should have been 90 min I tryed it out the next day and none of my parts bubble... anode or cathode... I'm trying to figure out what I'm doing wrong. It's set at 12 volts 2 amps.

Any help will be awesome.

Thanks,

Nick