Default Re: My 3'x3'x6' Oven project.

lol, now you have me confused. I understand the concept of putting the thermocouple in the pipe, but when do you put the parts in? Do you measure the oven temp with an IR gun and put the parts in at 400 deg then don't start timing the parts until the thermocouple reaches 400 deg?

Since I plan on running batches of smaller parts and batches of larger parts should I have two mounting locations for the thermocouple? One with a thicker walled tube for larger parts and one with a thinner walled tube for smaller parts?