jrow, i already posted a link to thier website on my first post and contacted them last week and they don't have any kind of coating on them.. no powdercoat, clear coat, anodized coating, protective coating on it..

1500 got rid of the spots when i tested it on some areas.. i think i'll be ok going down to 600 and no lower.. i'm still new on this aluminum buffing thing and i already spent a lot on cleaners nad polishers that i found out i never really needed..

what would effectively remove those sanding scratches? emery, tripoli or white rouge? i only have a dremel and a VSR drill to work with..