Thread: polishing frame
View Single Post
  #1 (permalink)  
Old 03-05-2008, 11:42 AM
dewie dewie is offline
Newbie
 
Join Date: Mar 2008
Posts: 2
dewie is on a distinguished road
Default polishing frame

Hey Guys,
My name is Duane and am new to the polishing world. I started with my Hayabusa mufflers and foot pegs and grab bar with good success. Then I started the frame. And I'm new to buffing wheels and different compounds. Here are the steps I did.
Gasket remover to eat the hard coating on the frame, vs oven cleaner
100 dry
150 dry
220 dry
320 dry
400 dry
600 dry
800 wet
1000 wet
1500 wet
2000 wet
Then onto wheels,
spiral sewn wheel with black emery
spiral sewn with red tripoli
loose with white compound.

I don't know what I'm doing wrong but there is micro scrathes and a haze all over it. any advise would be great. I tried to attach some pic's but they where to big, this is a link to a bike forum where I asked the same questions but they have pictures. I hope non members can access the page - http://www.extremebusa.com/extreme/s...386#post168386
Reply With Quote