yes, these pieces are being anodized after they are polished.



So, I think I'm going to skip sisal and then end with a flannel wheel and if that doesn't do it I'll just have to work something out with the customer.

Also, I only use white rouge on my loose cotton wheel yet the surface of the wheel is black, is this normal? If I remember right it turned black even when I first added white rouge to it.