Default Re: WeTDrEaM Oven Build. Step by Step

This is what it looks like after the upright studs were installed and the cross studs were installed. You can see in the pics I have the studs screwed in at the ends. I left room because after the oven is all framed in I am going to go back and drill holes and rivet next to them. After there is 2 fasteners holding each stud the unit will be much more rigid.
Attached Thumbnails
wetdream-oven-build-step-step-powder-coating-oven-017.jpg  wetdream-oven-build-step-step-powder-coating-oven-016.jpg  