I think you have a great idea! I also think you misinterpreted photos of other ovens. Most will use recirculating fans to do what you propose. They are simply mounted on the outside to remove the fan motor from the heat flow.

Venting fans are something different. These are used to cool the oven after a curing cycle. Care must be taken not to cool the PC too quickly though.