That 13.6 Volt power supply would not be a good choice, It does not have a variable output, and it won't operate in constant current (current source) mode. The dimmer won't work with this either.

The lamp dimmer idea will only work with an unregulated power supply, an ordinary battery charger is an unregulated power supply.

I'm glad your here Neilfj, I can use the help.