View Single Post
  #1 (permalink)  
Old 04-07-2002, 07:59 PM
drdarvocet drdarvocet is offline
Newbie
 
Join Date: Apr 2002
Posts: 1
drdarvocet
Send a message via ICQ to drdarvocet
Default Removing Nickel Plating

I have an old carbon steel putter that I am thinking about either nickel or copper plated. It currently has a nickel-plated finish that is in bad shape. How Should I go about removing the prior finish to get down to the original metal? Would the process the same for either plating I would use? Thansk in advance for your expertise and info.