Sometimes colors can be successfully mixed. We recently did a sample part for someone. We mixed a med. blue with a silver and ended up with a lovely silvery blue color. This won't always work; it depends on the powder.

As to the maximum part size that can be powder coated, that is limited only by your equipment size. Entire railroad cars are even coated with a graffiti-proof powder coating!