View Single Post
  #5 (permalink)  
Old 03-15-2008, 01:33 PM
Harleydad's Avatar
Harleydad Harleydad is offline
Metal Finishing Guru
 
Join Date: Dec 2006
Location: Wisconsin
Posts: 545
Harleydad is an unknown quantity at this point
Default Re: Extreme Chrome problem

Are you checking the part temp with an I.R. Temp gun or you just put it oven at 375 for 30 minutes. That 375 refers to the part temp.