Part not taking dye well
I've been having some trouble with this one part for a while now (an ego frame for you paintball guys). The weird part is that the first time I ran it I got a nice deep black, but there was one tiny little flaw so I decided to redo it. Now every time I run it it doesn't take dye very well at all.
Every time I strip it I get bad smut that is the same color as the previous anno and there are some streaks/blotches that only come off with heavy beadblasting. Also, I'm pretty sure it's not a bad connection since the voltage stays normal through the whole process and it's the only part I'm running.