Re: new to powder coating need help with oven
http://stores.ebay.com/Powder-Coating-Ovens-and-Supply
I make and sell the controllers to save electrical hassles. I think a few others on the board do also.
Gene
__________________
www.newfabco.com
http://stores.ebay.com/Powder-Coating-Ovens-and-Supply