You can use all kinds of media...Make sure you pay attention to your health on this one. Silica can harm you pretty bad. Wear a resperator with ANY media. With sand you need a real blasting hood. If you have a blast cabinet I still use a good quality paint mask. I use Black beauty 30/60 recyled 6 bucks for 50 lbs. I would use virgin 40/60 Black beauty for the cost and finish. AO is a really good media to use if you have the money.

No glass!