I used furnace cement and it seemed to be the cause of dirt in my powder. I got the rubberized silicon sealer by Rutland. It cures at room temp and will withstand 600 deg. So far, no problems and it stays put. I ran it around the seams and joints where the metal joined. I picked it up at Menard's, but am sure other place like that handle it.
Thanks JTW,

Any thoughts on the use of automotive high-temp silicone RTV as a sealer? It's easier for me to get in caulk tubes and works really well for things like header flanges, etc. Whadaya think?

SWPruett