Default High temp Powder coating Problems

Has any one had any luck with the high temp powder coating from Caswell? ......i brought in 23 parts off my new harley...to work .....were they powder coat all the time......and basically the coating came off in sheets...and the stuff that stuck....looked like ****! ....... the only thing i can think of is ..they didnt let it cure in the oven long enough? ......I read someones blog that said even silicone residue from the air compressor can cause it to not stick? ......which is really confusing to me.....since the High temp is supposed to be silicone based? .......Any help or suggestions would really help!!! .... i really dont have $3000 to replace the parts ..if the screw em up again !! Thanks