View Single Post
  #1 (permalink)  
Old 10-07-2003, 04:58 PM
buckeyevs buckeyevs is offline
Newbie
 
Join Date: Jul 2003
Posts: 25
buckeyevs
Default Polishing aluminum quickly?

Ok I have a vibratory tumbler and have run these parts through Course, Medium, and Fine ceramic triangles. Then metal polish treated corncob, each having a run time of 6 hours and the result is absolutely not what I would call polished. Is there a trick to using the corncob or should I abandon that procedure? Is there any other method of mass producing a polished finish that can be anodized? manual plishing just takes far to much of my time to be practical. Any other media for the tumbler that would do a better job than corncob? Any help would be very much appreciated.
Reply With Quote