Thread
:
Plug-n-plate
View Single Post
#
2
(
permalink
)
03-19-2008, 12:18 PM
crob241
Newbie
Join Date: Apr 2007
Location: hesperia, calif
Posts: 17
Re: Plug-n-plate
If you want to remove the gold, just polish it off. It is soft and thin and should come off with hand polishing, same for any brush plated finishes. thnx