I went to Lowes and bought an inline moisture separator for now. I can't believe the cost of the good air dryers
Any other ideas of why it might not be sticking to the part? I used the same process that i've used in the past. Degrease, Blast (AO), Clean Off, Iron Phosphate, then Rinse, Shoot.
Baz, you do amazing work! Your site is super nice and easy to work.
How did you get this finish? It looks awesome!