I'm using a Harbor Freight hobby gun. My ground was connected to the hanging hook.

This is my compressor...you can see the dryer I have sitting on top of the air hose. It's the first thing connected to the compressor. I drain it every morning when I get to the shop.


I'm gonna have to try that color...looks great!

Thanks, John