View Single Post
  #1 (permalink)  
Old 03-25-2008, 12:27 AM
tjespo22 tjespo22 is offline
Newbie
 
Join Date: Dec 2007
Posts: 27
tjespo22 is on a distinguished road
Default stripping powdercoat.

well i was originally going to give my stuff to a sandblasted but have read that its not good for quad/bmx parts (thats what im going to be doing most of the time) because it weakens the welds alot after a couple times of being stripped. what other ways are common that the pro's use? i have head something about "burning it off" ?

thanks
espo