More data on Copy Cad and Yellow Cad coloring
Fellow Platers:
In thinking more about my issues, I am hanging the bolts from thin brass wires into the solution. Do you suppose the ends are acting as anodes more and the bolts, with threads, need more time for the copy cad to take, so the yellow cad coloring will be uniform? Thanks Tom
|