Re: What are your thoughts on this VIBRATING METAL POLISHER?
I cannot get a mirror reflective finish from vibe tumbling, but the polish I get for anodizing is fine. I have a 35lbs capacity 1/2CuFt for finishing large amounts of small parts with a flow thru added in.
Your best bet is to get some corn cob and treat it with chromium oxide green powder yourself, then add in turbo brite tumbling paste and let them go for about 3 days, this will yeild a very nice result.
|