It's not their Industrial model, just the hobbyist model, so be careful if you plan on using it a lot. It also looks dusty and used in the picture.

We sell their industrial model at http://www.caswellplating.com/buffs/...y_tumblers.htm
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote