Default Re: Propane Oven - I know it's been asked

Quote:
Originally Posted by yyaarv View Post
I wasn't going to put the tank inside. I was goind to black pipe it to a tank outside. These units are only about $130 bucks so if I needed 5 of them that is no problem. I was just wondering if they would do the job?
These are infrared heaters without a blower. I think most of the larger ovens you will find have an outside burner with a blower. I sent you a pm on a few other contacts.